GB/T 18844.2-2018
ActivePlain bearings—Type, appearance and characterization,causes of damage to metallic hydrodynamic bearings—Part 2: Cavation erosion and its countermeasures
滑动轴承 液体动压金属轴承损坏类型、外观特征和原因分析 第2部分:气蚀及对策
Application Summary AI generated
This standard specifies the identification, characterization, and analysis of cavitation erosion damage in metallic hydrodynamic plain bearings, along with recommended countermeasures. It is applied in the design, failure analysis, and maintenance of rotating machinery such as turbines, compressors, and large engines where oil-lubricated bearings operate under high-speed, high-load conditions. The standard helps engineers diagnose cavitation-related failures and implement preventive measures to improve bearing reliability and service life.
Related Standards
JB/T 51110-1999
Internal Combustion Engines - Cylinder Head Gaskets - Product Quality Grading (Internal Use)
JB/T 51134-1999
Product quality grading of agricultural deep groove ball bearing
GB/T 5868-2003
Rolling bearings--Mounting dimensions
GB/T 4605-2003
Rolling bearings--Thrust needle roller and cage assemblies,thrust washers
GB/T 4199-2003
Rolling bearings--Tolerances--Definitions
GB/T 307.2-2005
Rolling bearings-Measuring and gauging principles and methods
GB/T 307.3-2005
Rolling bearings-General technical regulations
GB/T 307.1-2005
Rolling bearings-Radial bearings-Tolerances
Transparency note: The application summary and key sentences on this page were automatically generated by AI from the standard's original text. This content has not been human-verified and should not be used for compliance or regulatory purposes. Always refer to the official standard document from the issuing authority.